毛毡
|
尺寸 Size |
mm |
≥2mm,图纸有要求时按照图纸要求执行 When There Are Requirements On The Drawing, Follow The Drawing Requirements |
|
发泡实验 Foam Experiment |
|
毛毡不能与发泡料产生反应,不能结块 Felt Cannot React With Foam Material And Cannot Clump Together |
|
毛毡不能结块,应具有丝状纤维 Felt Should Not Clump And Should Have Filamentous Fibers |
||
|
观察泡料上粘贴痕迹,粘贴面积应大于80%Observe the adhesive Marks On The Foam Material, And The Adhesive Area Should Be Greater Than 80% |
||
|
克重 Grammage |
g/m2 |
≥180 |
|
拉伸强度 Tensile Strength |
MPa |
≥1.0 |
|
断裂伸长率 Elongation At Break |
% |
≥80%,图纸有要求时按图纸要求执行 When There Are Requirements On The Drawing, Follow The Drawing Requirements |
|
隔离纸克重 Weight Of Isolation Paper |
g/㎡ |
材质为淋膜牛皮纸,重量≥75;材质为绵纸,重量≥30g/㎡。图纸有要求时按图纸要求执行 The Material Is Coated Kraft Paper, With A Weight Of ≥ 75; The Material Is Cotton Paper, With A Weight Of ≥ 30g/㎡ . When There Are Requirements On The Drawing, Follow The Drawing Requirements |
|
环戊烷熏蒸 Cyclopentane Fumigation |
h |